Abstract
The surface to volume ratio is increasing due to the cost-driven reduction of the solar cell thickness thickness, which makes surface passivation a decisive factor for the final solar cell efficiency. Al2O3 have a high dielectric constant as a dielectric layer and have sufficient build-in nagative fixed oxide charge which generates an electric field. This field effect prevent the chances of minority carrier recombine at the surface which can greatly enhance the surface passivation. Meanwhile Atomic Layer Deposition (ALD) coating technology is developing rapidly in recent years, a film thickness can precisely control by number of cycles. Its good uniformity characteristics and an excellent aspect ratio so that today many companies used in the film manufacturing process. In this study, different thickness of ALD Al2O3 under different annealing conditions and PECVD SiNx are plated on n type Si wafers to examine the passivation effect. After that the samples are made into MOS structure to get the high-frequency capacitance-voltage data. The calculation of the doping concentration of the silicon substrate, the depletion zone width, the flat band voltage and fixed oxide charge will be found. The results show that annealing treatment and high temperature PECVD lead Al2O3 fixed oxide charge change from positive into negative, then the field effect passivation has improved significantly which is also reflected in the PCD effective carrier lifetime measurement of results and for covering the SiNx. The trend of lifetime and fixed oxide charge density versus different thickness of ALD Al2O3 are the same. This explains the good passivation effect is due to more fixed oxide charge in oxide layer. In addition, we observe that there are blisters generated at film surface. With increasing film thickness and number of heat treatment density blister appeared also increases but no direct effect on the effective carrier lifetime results.