薄膜 量子井態 功函數 表面能 角解析光電子能譜 微觀四探針電性量測 超導溫度 電子聲子耦合參數 thin film quantum well state work function surface energy angle-resolved photoemission spectroscopy microscopic four point probe conductivity measurement superconductivity transition temperature electron-phonon coupling constant
We measured work function of Pb thin films/Ge(111) from 1 to 13 ML. The work function shows a Bilayer oscillation with thin film thickness. Besides, the higher highest occupied quantum well state (HOQWS), the higher work function. A turning point of the bilayer oscillation was found near 11ML. Compare the work function with thermal stability of thin films, we found that the phase difference between work function and thermal stability is 1.62, which is close to the phase difference, 1/4 of periodicity, 1.57 predicted by free electron model. Another topic is the microscopic four-point probes (micro 4PP) conductivity measurement on Pb thin films. We measured the superconductivity transition temperature (Tc) of 3 ML, 4 ML, and 8 ML is 1.60 K, 3.65 K, and 5.21 K. We also measured the electron phonon coupling (EPC) of 6 ML and 8 ML Pb thin film by ARPES. The EPC of 6 ML and 8 ML QWS of Pb thin film is 1.09 and 1.27. From above results, we found that both the Tc and EPC of the Pb films are increasing with film thickness. It is concordant with many results found in similar systems. Finally, we made a comparison and discussion of superconductivity transition temperature by micro 4PP measurement and by EPC prediction.

Metrics

1 Record Views

Details

Logo image