摘要
In this study, a high entropy superalloy Al0.2Co1.5CrFeNi1.5Ti0.3Nb0.05 was used as the substrate, and pack cementation was employed to perform aluminized and aluminized-siliconized treatments. After the formation of coatings, the growth kinetics, microstructures, and high-temperature oxidation resistance were investigated. The aluminide coating exhibits a three-layered structure—an Al-rich layer, a β-Al(CoFeNi) layer, and an interdiffusion layer—driven by high- and low-activity diffusion. In the aluminized-siliconized coating, Si internally segregated to precipitate Fe2Si rather than forming a protective Si-rich layer. Consequently, its oxidation resistance still relied on the α-Al2O3 layer. Due to a lower Al content, the aluminized-siliconized coating showed inferior oxidation resistance, evidenced by higher isothermal and cyclic weight gains (1.573 mg/ cm2 and 2.036 mg/ cm2) compared to the aluminide coating (0.899 mg/ cm2 and 1.355 mg/ cm2).
•A growth kinetic equation (Q = 34.03 kJ/mol) was established for pack aluminized coatings on AlCoCrFeNiTiNb high-entropy superalloy.•The aluminide coating exhibits a three-layer structure driven by combined high- and low-activity diffusion, whereas internal Fe2Si segregation in the aluminized-siliconized coating suppresses the low-activity outward diffusion.•Aluminide coating maintains a higher Al content, forming a continuous and protective α-Al2O3 layer at 1100 °C.•Aluminizing provides superior isothermal and cyclic oxidation resistance at 1100 °C compared to aluminized-siliconized coating, achieving an overall oxidation performance improvement of ∼38.2%.