Ni-Al-Cr superalloy as high temperature cathode current collector for advanced thin film Li batteries
期刊文章   開放取用(OA)

Ni-Al-Cr superalloy as high temperature cathode current collector for advanced thin film Li batteries

Alejandro N. Filippin, Tzu-Ying Lin, Michael Rawlence, Tanja Zünd, Kostiantyn Kravchyk, Jordi Sastre-Pellicer, Stefan G. Haass, Aneliia Wäckerlin, Maksym V. Kovalenko 和 Stephan Buecheler
RSC Advances, 卷.8(36), 頁碼.20304-20313
2018

摘要

Chemistry (all) Chemical Engineering (all)
To obtain full advantage of state-of-the-art solid-state lithium-based batteries, produced by sequential deposition of high voltage cathodes and promising oxide-based electrolytes, the current collector must withstand high temperatures (>600 °C) in oxygen atmosphere. This imposes severe restrictions on the choice of materials for the first layer, usually the cathode current collector. It not only must be electrochemically stable at high voltage, but also remain conductive upon deposition and annealing of the subsequent layers without presenting a strong diffusion of its constituent elements into the cathode. A novel cathode current collector based on a Ni-Al-Cr superalloy with target composition Ni <sub>0.72</sub> Al <sub>0.18</sub> Cr <sub>0.10</sub> is presented here. The suitability of this superalloy as a high voltage current collector was verified by determining its electrochemical stability at high voltage by crystallizing and cycling of LiCoO <sub>2</sub> directly onto it.

檔案與連結 (1)

url
https://doi.org/10.1039/c8ra02461h檢視
已出版(紀錄版本) 開放

相關連結

指標

1 檢視次數

詳細資料

Logo image