Logo image
Tolerance assessment and crack growth of chloride-induced stress corrosion cracking for Chinshan dry storage system
期刊文章   開放取用(OA)   同儕審查

Tolerance assessment and crack growth of chloride-induced stress corrosion cracking for Chinshan dry storage system

Wen-Yu Wang, Yung-Shin Tseng 和 Tsung-Kuang Yeh
Progress in nuclear energy (New series), 卷.147, 頁.104210
01/05/2022
Web of Science ID: WOS:000805469300001

摘要

Nuclear Science & Technology Science & Technology Technology
Evaluating the susceptibility of canister used in Chinshan Independent Spent Fuel Storage Installation (CSISFSI) to chloride-induced stress corrosion cracking (CISCC) has been an aging management plan in an initial license period of 20 years. The presence of concentrated chlorides, temperature and relative humidity, and sufficient weld residual stress are the three key environmental conditions for atmospheric CISCC. A single 2-D model was used to simulate natural exposure of austenitic stainless steel (SS) of SS304 and SS304L dry storage system (DSS) for transportable storage canister (TSC). This model will calculate the temperature on the TSC surface based on CFD method. This study estimated RH and DRH on the TSC surface by the realistic environmental conditions (e. g., ambient RH, ambient temperature, and the temperature on the TSC surface) after 1st, 10th, and 20th years, respectively. The flaw tolerance to part-depth (PD) and through-wall (TW) critical flaw were evaluated, and the two-phase CGR induced by CaCl2 or MgCl2 of the TSC surface under 0.18 m height were predicted. The results show that the fastest CISCC CGR was on the bottom induced by CaCl2 in the 20th year, and the slowest CGR was at the 0.18 m of TSC induced by MgCl2 in the 10th year. The two-phase CGR trends were very close if the deliquescence threshold had been considered under different environmental conditions.

檔案與連結 (1)

pdf
1-s2.0-S0149197022000889-main4.37 MB下載檢視
開放存取(OA)

相關連結

指標

1 檢視次數

詳細資料

Logo image