Transient and steady-state nanoindentation creep of polymeric materials

Chien-Chao Huang, Mao-Kuo Wei and Sanboh Lee
International Journal of Plasticity, Vol.27(7), pp.1093-1102
07/2011

Abstract

Nanoindentation creep Polymer Power-law creep Viscoelasticity
The transient and steady-state nanoindentation creep of polymeric materials was investigated. The creep model is used to explain the experimental data of transient and steady-state creep dominated by viscoelastic deformation and power-law creep deformation, respectively. The Burgers viscoelastic model was used to interpret the transient creep in polymers under nano-indentation. Explicit expression for the displacement of transient creep was derived using the correspondence principle of linear viscoelasticity theory. The power law of strain rate-stress relation was used to explain the creep displacement during the steady state. Three polymers of poly(methyl methacrylate), hydroxyethyl methacrylate copolymer, and the fast-cure acrylic resin were used to measure the nanoindentation creep. The transient creep data are in good agreement with the predictions from the Burgers viscoelastic model. The creep displacement is mainly attributed to the viscous flow of the Kelvin element, and the computed values of viscosities (η 1,c , η 2,c ) increase with decreasing preloading rate. By comparing the steady-state creep data with the power law of strain rate-stress relation, the stress exponents for the above polymeric materials were quantitatively determined. © 2010 Elsevier Ltd. All rights reserved.

Metrics

1 Record Views

Details

Logo image