摘要
A method for preparing a biodegradable polyester elastomer includes a following steps comprising: dissolving a predetermined amount of titanium dioxide in an aqueous mixture of sulphuric acid, DI water, and ethanol to form a first solution; refluxing the first solution in a silicone oil bath and a stirring speed of 300-450 rpm at a temperature of 90-100° C. to form a second solution; preparing a solid superacid catalyst by drying, grinding and calcining sulfated titania and using this catalyst to produce a biodegradable polyester elastomer.